Conductive coating (CM0485115) provides a high-conductivity solution for dissipating static on aluminum and composite aircraft.
Photo Credit: Sherwin-Williams Aerospace Coatings
Sherwin-Williams Aerospace Coatings has added an aerospace conductive coating (CM0485115) to its line of undercoats, enabling aircraft owners to impart conductivity onto aluminum and composite substrates. The coating offers high conductivity to nonconductive substrates by producing an antistatic conductive film on their surfaces with a resistivity of 0.1 to 100,000 ohms per square meter to help static charges dissipate from antennas and radomes. The company says the coating is designed with excellent adhesion and offers excellent fluid resistance.
Conductive coating (CM0485115) is designed to work with Sherwin-Williams topcoat systems. Using a 1:1 mix ratio, the product is simple to mix and apply. It is compatible with all non-electrostatic spray equipment and can be applied onto pre-primed aluminum and composite substrates to achieve high conductivity. The company notes that the best results are achieved when the conductive coating is applied in one singular, continuous closed film or one cross coat. The application can happen in a range of environmental conditions, and the coating can be air cured or force dried, providing flexibility for applicators. Drying times vary based on the dry film thickness.
“As composite substrates continue to grow in popularity in the aerospace market, it’s important for our customers to have ready access to a robust conductive coating that can meet their requirements for functionality, durability and ease of application,” says Julie Voisin, market segment manager, aerospace, original equipment manufacturer interior and commercial vehicle refinish. “Our new conductive coating is a perfect complement to our product offering and commitment to deliver high-performing products to the aerospace marketplace.”
Related Content
-
NADCAP Shop Digitizes to Eliminate Paper Trail
Customizable ERP software has transformed a 27-year-old manual metal finishing job shop into a state-of-the-art paperless company with full digital traceability in about 10 months.
-
AkzoNobel Uses VR for Training Airline Apprentices
The virtual reality technology provides a paint booth and spray gun that enables trainees to work and master their skills without losing parts in the process.
-
Top Shop’s Journey to Building a Unique Brand
Since this new Ohio plater took over the space and assets of a former plating business, it is intentional about setting itself apart from prior ownership.