ELECTROPLATING CLINIC

Electroplating

Preventing Dark Streaks in Trivalent Chromium

Matt Schario from Columbia Chemical explains what is the likely cause of these streaks and patterns, and how to prevent this from happening.  
#asktheexpert

Electroplating

Finding Correlations to Salt Spray and UV Protection Hours

Bob Hohn with Assured Testing Services says it is often difficult to equate test duration to actual years of field service.
#asktheexpert

Anodizing

Fixing Excessive Brightener Consumption From Dull Work In Alkaline Non-Cyanide Zinc

Although great strides have been made over the last 30 years in the development of alkaline non-cyanide zinc processes, Asterion’s Graham Torr says not all “modern” systems are created equal.
#asktheexpert

Electroplating

Fixing Salt Spray Failures After Passivating, Baking

This is a common challenge faced by many acid zinc platers who Mark Adams from Columbia Chemical says perform hydrogen embrittlement relief on acid zinc plated fasteners.
#asktheexpert

Electroplating

Measuring Hardness and Wear in Electroless Nickel Coatings

Rich O’Brien from Bales Metal Surface Solutions says advances in coatings science have led to the development of multiple choices for surface finishes beyond hard chrome and electroless nickel.
#asktheexpert

Electroplating

Automate Your Brush Plating Operation

Derek Kilgore from Sifco ASC says the brush plating operation can be mechanized, semi-automated or even fully automated.
#asktheexpert

Electroplating

Determining the Proper Material for an Electroless Nickel Plating Tank

The stability of your electroless nickel (EN) bath may require one type of tank over another, says Mike Aleksinas of MetalChem.
#asktheexpert

Electroplating

Summary Report on USCAR Field Test for Trivalent Chromium

Mark Schario from Columbia Chemical explains USCAR’s multiyear project to determine how various trivalent chromium systems would perform in the real world.
#asktheexpert

Powder Coating

Using Alternatives in Pretreatment Baths for Degreasing

Effective cleaning at low, even ambient temperatures, is possible, says Atotech’s Brandon Lloyd, and creates a safer work environment and reduces energy demands.
#asktheexpert #energy

Electroplating

Phosphorus Copper Anodes for Acid Copper Plating

Copper anodes produced from pure copper cathodes will result in a copper purity of greater than 99.99% copper, including silver and the alloyed phosphorus, according to Univertical’s André Depew.
#asktheexpert