Pretreatment for Powder Coating
Phosphate Coating Weights & Powder Thickness
How much will the corrosion performance of a component be affected if the coating weight is reduced from 120 to 80 GSM?
Read MorePowder Coating Hot-Dipped Galvanize
Do you know the procedure for powder coating galvanized steel?
Read MoreOn-site Powder Color Match
Is there any powder process where we can mix colors instantly and match color shades?
Read MoreEpoxy/Polyester Hybrid
Can a hybrid powder provide enough UV protection to be used for an outdoor application?
Read MoreCoverage of Powder
I would like to know the best method to measure the coverage of a powder in a production line.
Read MoreWhat Temperature Profiling System is Right for Me?
Today, profiling systems that are both sophisticated and easy to use can give a clear pass/fail finding, document regulatory compliance, let operators know when and where their ovens are trending out of acceptable limits or show that a process is within suppliers’ or customers’ specifications.
Read MoreSchools of Thought: More colleges offering programs in coatings
Employers such as 3M, Valspar, Bobcat, DuPont and Caterpillar routinely drop into classrooms at NDSU, scoping out a new hire to develop the next top coating compound or new corrosion-resistant material.
Read MoreAdhesion on Galvanized Steel
We just took on a new job for some parts that are hot-dipped galvanized and we are having big problems with adhesion failure.
Read More