sales
Chromium Plating on Aluminum
Can you supply me with a procedure for successfully plating chromium on aluminum?
Read MoreEpoxy Peeling Problem
After running the parts through a sterilization cycle, I lose the bond and the epoxy—it can be picked off with your fingers.
Read MoreA Valuation Victory for the Good Guys
First, a simple question: How much would you pay for property that is worth $100,000, if you had to spend $25,000 (to fix it, commissions, special taxes or whatever) before collecting your $100,000?
Read MoreA Hunt for the Elusive Surface Finishing Economic Forecast
During a 30-day period this year, I pulled the following headlines related to the U.S. economy from various periodicals.
Read MoreCurrent Density Revisited
Question: Anodizers constantly raise the question of anodizing (sulfuric acid) by current density vs. voltage.
Read MoreBurned Chrome Deposits
What are some of the causes of chrome burn? How can I eliminate this problem?
Read MoreCyanide Copper Strike Bath
We want to replace our cyanide copper strike bath with a non-cyanide based strike bath. Are there any such baths available, and do they work?
Read MoreRust on 17-4ph
Could the customer’s rust be the thermal treating or just poor passivation, and to what extent can these parts be expected to rust if they are processed correctly but subjected to extreme conditions?
Read More