Published
Works of art in black oxide
Cleveland Black Oxide assists local artist
It’s not often that artists seek out black oxide finishing suppliers but when they do, the results can be quite dramatic -- and Cleveland Black Oxide can boast that its work is seen in the finest galleries.
Artist and sculptor Anne Lindberg of Kansas City, MO has her work widely exhibited in the U.S. and throughout the world. Some years ago Anne began experimenting with projects using piano wire and stainless steel wire and rods of varying thickness. She fastened these wire rods, sometimes thousands of them, onto a backing material in varying shapes and densities giving a striking three dimensional effect. Her work is displayed over a large area in the gallery and invites the viewer to apply their own interpretations. She often combines wood or other material with the wire to add dimension and achieve a particular visual effect. The trick, she says, is to have the rods bend with just the right arc.
In experimenting with paint and other surface treatments, Anne discovered that black oxide would give the flat black color she was searching for without altering the thickness of the stainless wire or its bending properties. Unlike paint or powder coating, black oxide is a surface conversion process and does not alter the physical dimensions of the part. Finishes can range from flat to shiny depending on surface conditions and post process treatments.
David Tatham, president of Cleveland Black Oxide says: “We see all kinds of parts come in for black oxide but this has to be one of the most interesting and beautiful applications. We’re proud that Anne chose us to be a partner in her work.”
For more information on black oxide finishes, visit www.clevelandblackoxide.com
To see more of Anne Lindberg’s work, visit www.annelindberg.com
Related Content
-
Finishing Systems Provider Celebrates 150 Years, Looks to Future
From humble beginnings as an Indiana-based tin shop, Koch Finishing Systems has evolved into one of the most trusted finishing equipment providers in the industry.
-
Chicago Anodizer Emphasizes Relationships as Key to Growing Business
Chicago Anodizing Company continues to grow its 75-year old business by investing in its people and partners, and by embracing new technologies.
-
Cleaning, Pretreatment to Meet Medical Specs ISO 13485 or FDA 21 CFR820
Maximilian Kessler from SurTec explains new practices for industrial parts cleaning, metal pretreatment and decorative electroplating in the medical device industry.