Pretreatments

Breakthrough in Total Closed Loop Recycling

At Honeywell CPG Greenville, Total Closed Loop Recycling is not a dream or a concept anymore…it is a reality in the day-to-day plant process...

Read More

Rust Prevention Steel Tubes

Question: We powder coat welded steel tubing (ANSI 1008-1010). We have a five-stage washer followed by a dry-off oven before we apply powder coating.

Read More

More Adhesion Troubles

Question: We are a die caster who has some of our castings powder coated.  We are experiencing an adhesion problem with some of the castings we supply to a certain customer.  The castings are all run with the same process parameters, but some of the castings do not pass a crosshatch test and some from the same batch do.  We have obtained samples of this problem, and I am hoping that you can provide us with the name of a lab that could answer what may be on these castings (if anything) or what process is adversely affecting the adhesion.

Read More

Rusting after Vibratory Finishing

Question: We are the leading company in our country in mass-finishing.

Read More

Improving Metal Pretreatment

Improving Metal Pretreatment Question: We are one of the leading two-wheeler manufacturers in our country and produce more than one million bikes a year.

Read More

Painting Aluminum

Question: We are a small ornamental iron shop.In an effort to offer a more durable outside railing to customers, we have been manufacturing our ornamental iron designs from aluminum using traditional structural, just as with wrought iron, one-inch-square tubes, one-half-inch punched channels for framing, one-half-inch square solids for balusters, molded top rail or a channel for a top cover.

Read More

Painting Over Zinc

Question: I currently manufacture a part out of cold rolled steel.

Read More

Pretreatment Over Pretreatment, Part 2

Question: Your response to “Pretreatment Over Pretreatment” in the February Painting Clinic should be amended to warn him that running aluminum through an Iron phosphate spray washer would make the sludge in the washer a hazardous waste (according to an earlier comment you made about a year ago). I believe the problem is created by the definition of acid washing of aluminum is a categorical hazardous waste (by EPA definition). When he cleans the washer, all the sludge that is normally sent to the landfill or flushed down the sanitary sewer would be considered an illegal disposal of hazardous waste.

Read More

Pretreatment over Pretreatment

Question: We are considering forming an assembly and then painting it rather than painting the individual parts before assembling.

Read More

Minimizing Rust, Part 2

Question: I read your clinic in the December issue and would like to point out factual errors in the section titled, “Minimizing Rust.” At the end of your response, you have given the parameters necessary to achieve a particular result in the salt spray test.

Read More
find masking products online
New Acid-Free Bright Nickel Process
The Finishing Industry’s Education and Networking Resource
Pretreatment Washer and Finishing Equipment
Heatmax Heaters ad with immersion heaters
Filtration Systems
plating and surface finishing additives
Metal Pretreatment Technology
cfs masking