marketing
UV Powder Coating
UV Powder Coating Question: I am attempting to find out as much as possible about UV powder coating, including the process itself and the equipment required.
Read MoreWrinkle Powders
Question: I have a customer that is trying to process a wrinkle powder in a catalytic IR oven with poor results.
Read MorePowder Chipping off Glass
Question: We have a powder coating system that coats perfume bottles.
Read MoreWhat Causes Outgassing?
Question: I read with interest your comment regarding powder coating over galvanized surfaces in the April issue of Products Finishing.
Read MoreVacuum Deposition of Selenium
Question: We vacuum deposit selenium on 3003 and 6063 aluminum alloy drums for copy machines.
Read MoreOn My Mind: Powder Coating Trends
For those of you that didn't make it to the Powder Coating '00 show, I thought I would fill you in on the latest trends.
Read MorePlating Zinc over Heat Treating
I am not able to plate zinc over an area that has been heat treated. Any suggestions?
Read MorePreventing Oxidation and Decarburization
Question: Can I prevent oxidation and decarburization during hardening of 1055 steel at 860C with super-heated steam at 550C using pretreatments?
Read More