I’m sure there is more than one material used to make paints flat. Does any one stand out as being more resistant to burnishing? Are different agents more efficient in their ability to create a flat finish? What would be your formula for the perfect clear coat?
Read MoreHVLP For Automotive Refinishing
If you were to advise a painter who has to work with high-solids, low-VOC coatings and/or water-based paints and primers on how to select an HVLP, what would you suggest he look for? What selection criteria should he use?
Read MoreCracked Chrome
We have a problem with our hard chrome plate. A customer has stated that the hard chrome we are plating has “too many cracks” and the cracks are “too deep.” Where can we obtain additional information on how to control the cracking?
Read MoreAdhesion Failure as Time Goes By
What failure mechanism could likely trigger this? What are the material conditions that might be contributing to this?
Read MoreCQI-11 Assessment
Recently our company was asked when we will implement the CQI-11 Plating System Assessment Program. Before we can do anything we must find out what it is. Do you have any information on this program?
Read MoreFinishing System Durability
While the specific paint chemistry can clearly have dramatic impact on the durability of the finished component, the use of effective surface cleaning and conversion coating practices may actually have an even greater impact. If end users and coatings applicators are looking to improve paint adhesion and corrosion resistance, it is critical to consider the surface preparation of the component.
Read MoreFrench Revolution
An urban bike Movement is sweeping Paris, and French custom coater Solyap is riding the wave