Dassault Aviation Qualifies PPG Ecoat Aerospace Primer
Qualification to DGT153703 enables Dassault subcontractors to produce parts for the aircraft manufacturer using the chrome-free PPG e-coat primer.
![ppg ecoat tank](https://d2n4wb9orp1vta.cloudfront.net/cms/PF/Blog/AEROCRON_PPG_2.jpg;maxWidth=600)
PPG has qualified its proprietary Aerocron electrocoat aerospace primer at Dassault Aviation for application to structural aircraft parts for corrosion resistance. Qualification to DGT153703 enables Dassault subcontractors to produce parts for the aircraft manufacturer using the chrome-free PPG e-coat primer.
According to Daniel Bencun, PPG segment manager for aerospace coatings in the Europe, Middle East and Africa region, the Dassault qualification demonstrates growing interest in the advantages of PPG’s ecoat primer.
“Throughout its history, Dassault has been an innovator and aviation industry leader, and qualifying Aerocron primer shows Dassault’s continued commitment to technological advancements and the environment,” Bencun said. “In addition to its many application and performance benefits, Aerocron primer is chrome-free and water-based, and it reduces emissions as well as waste-treatment requirements.”
In the e-coat process, metal parts are immersed into the electrically charged Aerocron primer bath. Compared with traditional spray primer application, PPG’s e-coat process provides better corrosion protection, more uniform application, and less coating weight for cost savings and enhanced aircraft fuel economy. Product utilization with Aerocron primer is significantly higher with no overspray, eliminating related worker exposure and producing near-zero waste.
“Dassault aircraft operators will benefit from the reduced weight of coated parts and superior corrosion resistance with Aerocron primer,” Bencun said. “While it is difficult to spray on a primer with a consistent coating thickness, Aerocron primer achieves a uniform thickness even on hidden and recessed areas of a part, a significant advantage important within the aerospace industry. Weight savings can be about 30 percent for flat parts and up to 75 percent on complex-shaped parts.”
Aerocron primer is also qualified to SAE International’s Aerospace Material Specification 3144 for anodic electrodeposition primer for aircraft applications.
PPG’s global aerospace business offers coatings, sealants, transparencies, packaging and application systems, and transparent armor, as well as chemical management and other services. For more information, visit ppgaerospace.com.
Related Content
-
Novel Wastewater Treatment Targets Micropollutants
Swiss wastewater treatment technology provider Oxyle specializes in advanced wastewater treatment for removal of highly persistent micropollutants such as PFAS.
-
Explore Cleaning Chemistry, Metal Finishing Applications and Wastewater Treatment Solutions
Hubbard-Hall Celebrating 175 years of excellence, Hubbard-Hall presents chemistry and equipment.
-
In-House Blackening of Ferrous and Non-Ferrous Metals
Process satisfies customers’ shipping requirements while meeting stricter water regulations in times of drought.