Question: We manufacture 0.050 inch aluminum parts that require stainless steel PEM standoff inserts.
Question:
We manufacture 0.050 inch aluminum parts that require stainless steel PEM standoff inserts. We powder coat the products with a thin film coating to achieve a class A surface finish. What do you recommend for a quick and easy filler material to hide the heads of the inserts? V.S.
Answer:
Our readers like to use Lab-Metal, manufactured by Alvin Products. It is an aluminum filler that is both conductive and sandable. It has no problem handling the cure oven temperatures required for powder coating. They are listed on PF Online (http://www.pfonline.com/suppliers.html)or in the 2003 Products Finishing Directory and Technology Guide.
Related Content
-
Products Finishing Reveals 2023 Qualifying Top Shops
Each year PF conducts its Top Shops Benchmarking Survey, offering shops a tool to better understand their overall performance in the industry. The program also recognizes shops that meet a set of criteria to qualify as Top Shops.
-
Curing Oven Basics
Simply heating up the substrate does not cure the coating. There are many variables to consider when choosing the best cure oven for your application...
-
Reduced, Reused and Recycled Powder Coatings Are the Future
They say necessity is the mother of invention, and with millions of pounds of powder coating going into landfills a year, these two companies have found novel approaches to dealing with this waste stream.