PPG Aerospace Donates Coatings To Restore F-4
Jet on display at the New England Air Museum was restored with coatings and technical talent donated by PPG Industries
![](https://d2n4wb9orp1vta.cloudfront.net/cms/PPG_Paint_22_0815_aaa.jpg;maxWidth=600)
Kevin Lee, second from right, PPG senior account manager, aerospace; Jerry Roberts, NEAM executive director; Jim McGuire, restoration technician and an NEAM volunteer; and Kim Jones, NEAM board member and volunteer.
An F-4 Phantom fighter jet on display at the New England Air Museum was restored with coatings and technical talent donated by PPG Industries’ aerospace business to honor the jet’s U.S. Air Force service during the Vietnam War.
PPG donated high-solids Desothane HS/CA 8211 military and defense topcoat in camouflage, Desothane HS/CA 8800 topcoat in gloss white and Desoprime HS/CA 7700 primer. Kevin Lee, PPG senior account manager, aerospace, provided the technical talent and a personal connection to the aircraft manufacturer, McDonnell Douglas.
NEAM volunteer and restoration technician Jim McGuire contacted Lee, with whom he had worked in the past, to ask for PPG help in repainting the F-4, which is on loan to the museum from the U.S. Air Force. McGuire wanted it restored with its paint scheme from December 1972, when the aircraft was flown in a mission that downed an enemy MiG fighter jet. He knew what it looked like from a photo provided by the mission’s pilot and copilot.
![](https://d2n4wb9orp1vta.cloudfront.net/cms/PHOTO PPG Aerospace 33.jpg;maxWidth=600)
“I wanted to use the true military coatings that met the federal standards,” he said.
The assistance by Lee proved to be serendipitous. “My first experience in the aerospace industry came back in 1978 at McDonnell Douglas, in Tulsa, Oklahoma, where we completely refurbished the F-4 aircraft, including repainting.”
Lee selected PPG coatings that would provide a durable system with good ultraviolet (UV) protection that should retain its gloss and color for years. “This would most likely be the last time this historic airplane is renewed,” he said.
![](https://d2n4wb9orp1vta.cloudfront.net/cms/PHOTO PPG Aerospace 44.jpg;maxWidth=600)
McGuire and a team of volunteers painted the aircraft with Lee’s guidance. McGuire credited Lee and the financial and technical support from PPG for the restoration’s completion. “Words can’t describe the immense pride the crew and I take in having been able to get the lady back in her rightful colors and restore the essence of what this plane was and is,” McGuire said.
“The project was an amazing success,” Lee said, adding, “I worked for McDonnell Douglas for 16 years on the F-4, F-15 and F-18 fighter programs. To this day, for me, there is not a more beautiful airplane in the sky at 600 miles per hour than the F-4.”
The restored F-4 was unveiled this summer for a Vietnam 50th commemoration exhibit at the museum, where it will be on display through September.
PPG Aerospace is the aerospace products and services business of PPG Industries. PPG Aerospace – PRC-DeSoto is the leading global producer and distributor of aerospace coatings, sealants, and packaging and application systems. PPG Aerospace – Transparencies is the world’s largest supplier of aircraft windshields, windows and canopies. For more information, visit www.ppgaerospace.com.
Related Content
-
Caplugs Acquires Safeplast to Expand Solutions for Hose Protection
Caplugs acquires Safeplast as part of the company's efforts to expand hose protection capabilities.
-
Masking Solutions for Medical Applications
This article from Custom Fabricating & Supplies answers the question about how to break into the medical market with the masking process.
-
High Temp Alignment Masking Discs
Designed with printed alignment “target” rings for easy application, PCX-SH Series powder peel green discs from Caplugs ensure pinpoint accuracy when centering over any hole.