The Role of Surface Finishing in Modern Manufacturing: Trends and Best Practices
The entire manufacturing process for any part can benefit from considering the final finish early in the process. This article discusses trends in surface finishing with the goal of facilitating better communication with potential partners.
The fall trade show season offers numerous opportunities, such as the International Manufacturing Technology Show (IMTS), to explore where areas of manufacturing intersect. Increasingly, manufacturing professionals in all areas of the process chain are learning the importance of considering the final finishing of parts at earlier stages of the production process. The traditional approach of merely machining parts and sending them to a metal plater is outdated and should be left in the past. To achieve the highest quality, it’s essential to collaborate closely with every partner in the process chain, including surface finishing experts.
What are the current trends when it comes to surface finishing? Industry professionals are focusing on several key areas that shouldn’t come as a surprise.
![robots perform surface prep operations on a vehicle component](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/pf/2024-pf/0824pf-graymatter1.jpg;maxWidth=720)
GrayMatter Robotics provides artificial intelligence (AI)-driven software designed to enable robots to program themselves to perform surface finishing and surface prep operations for a wide variety of part sizes and shapes.
Source: GrayMatter Robotics
1. A.I., machine learning and IoT solutions
Much like other areas of manufacturing, finishers and coaters are seeking ways to streamline their processes. Today, finishers are increasingly exploring robotics, artificial intelligence and machine learning to tackle challenges such as workforce shortages, quality control and repeatability.
Historically, finishing operations have been slower to adopt IoT and automation solutions due to the high mix of parts typically processed by job shops, but various factors including workforce trends and demands for environmentally responsible and sustainable processes are accelerating the need to find new efficiencies.
Discover how one company is using A.I. to make finishing processes for a high mix of parts of varying geometries as easy as the push of a button. short.pfonline.com/graymatterAI
![3D printed lattice cubes](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/PF/2024-PF/0824-pf-repliform-5.jpg;maxWidth=720)
These lattice cubes were 3D printed from clear resin using stereolithography, then coated by RePliForm with electroless nickel, copper, and layers of ductile and hard nickel to improve their compression performance.
Source: Additive Manufacturing
2. 3D Printing
Additive manufacturing is growing exponentially. As this technology continues to move from the realm of R&D and short run production to full scale production, an increasing number of fabricators are looking to various finishing methodologies to not only protect parts or provide aesthetics, but in some cases to increase functionality.
Check out a story about how one company is using electroplating to enhance the physical properties of additively manufactured parts. short.pfonline.com/repliform3D
![Electric vehicle charging](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/PF/2024-PF/0824-pf-enev.jpg;maxWidth=720)
EVs present exciting new opportunities for additional growth of the use of electroless nickel plating in the automotive market for several critical components.
Source: Getty Images
3. Electroless Nickel Plating and EVs
The advent of electric vehicles (EVs) seems to have finally arrived. With a growing number of automotive OEMs investing in new capabilities to grow their EV and hybrid offerings, finishes will be needed for a range of parts from electrical motor components to batteries.
One example is electroless nickel (EN) plating. EN has been used in the automotive industry for decades. Applications include piston heads, carburetors and fuel injection components, slip yokes and transmission components. Today, EVs present exciting new opportunities for additional growth of EN in the automotive market with the finish being used for several critical components used in electric vehicles.
Learn more about the role EN is playing in the developing EV market: short.pfonline.com/ENandEV
![powder coating overspray](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/PF/2024-PF/0824-pf-recycle-ik-incoming-powder.jpg;maxWidth=720)
Powder coating overspray can be reclaimed and reused.
Source: Innovakote
4. Environmental Considerations
Contrary to some perceptions, environmental concerns are a priority in the finishing industry. As one of the most heavily regulated sectors in manufacturing, compliance is essential for the industry's sustainability. For years, metal finishers have been engaged in negotiations with environmental groups to address issues related to air quality and wastewater treatment. The industry has been proactive in seeking alternatives to potentially harmful hexavalent chromium finishing technologies, exploring safer options like trivalent chromium-based processes. The evolving regulatory landscape will continue to influence the available finishing technologies and their application methods.
This Products Finishing Ask the Expert column, discusses the environmental considerations driving some of these regulations: short.pfonline.com/hextotrichrome
In terms of coatings, powder coating has always been a low volatile organic compound (VOC) approach to coating parts, and powder overspray is a reclaimable material. Despite its already environmentally-friendly nature, new ways of making powder coating even more sustainable are being explored.
Check out this story about two companies that have found novel approaches to reclaiming powder. short.pfonline.com/reclaimpowder
![electroplated 3-D printed radar array](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/PF/2024-PF/0824-pf-arraylr.jpg;maxWidth=720)
This 3D printed radar array is PAEK plated with layers of copper and electroless nickel using a plating on plastic activation chemistry known as GreenPOP.
Source: Alliance Finishing and Manufacturing
5. Plating on Plastics
Plating on plastics (POP) isn’t new. Electroplating on plastic typically involves the process of depositing a thin layer of metal onto a plastic substrate using an electrochemical process after first preparing the plastic for the metal to adhere. Advances in plating on plastics, as well as the introduction of new materials aimed at producing lightweight parts are creating opportunities beyond traditional POP applications, which are often decorative in nature. Today POP is being explored for use in diverse industries including aerospace, automotive and electronics. The ability to electroplate on high performance resins, lightweight composites and additively manufactured parts opens new avenues for innovation, making plating on plastic an option for enhancing functionality of parts in addition to providing esthetics.
Learn more about new innovations in plating on plastics: short.pfonline.com/GreenPOP
Finishing today and tomorrow
The finishing industry is integral to the broader manufacturing landscape. Consumer needs and buying trends shape not only what we produce but also the methods we use. To ensure the highest quality for your parts, engage with your surface finishing partners early in the production process. Leverage their expertise to achieve the best possible surface finish, aligning with industry standards and consumer expectations.
Related Content
ECOAT24 Issues Call for Speakers
Don't miss your chance to apply to speak at ECOAT24. Submit your abstract by June 26, 2023.
Read MoreWorkforce Education is Never Finished
Educational initiatives in the industry offer training/learning opportunities for professionals who are entering the industry to seasoned employees as well as introductory programs for high school and college students.
Read MorePowder Coating Week 2023 Moves Industry Education Forward
Powder Coating Week 2023 offers can’t-miss powder coating industry education, networking opportunities.
Read MoreCelebrating Powder Coating
Products Finishing reflects on Powder Coating Week 2023 and the importance of powder coating in the finishing industry.
Read MoreRead Next
Education Bringing Cleaning to Machining
Debuting new speakers and cleaning technology content during this half-day workshop co-located with IMTS 2024.
Read MoreEpisode 45: An Interview with Chandler Mancuso, MacDermid Envio Solutions
Chandler Mancuso, technical director with MacDermid Envio discusses updating your wastewater treatment system and implementing materials recycling solutions to increase efficiencies, control costs and reduce environmental impact.
Read MoreA ‘Clean’ Agenda Offers Unique Presentations in Chicago
The 2024 Parts Cleaning Conference, co-located with the International Manufacturing Technology Show, includes presentations by several speakers who are new to the conference and topics that have not been covered in past editions of this event.
Read More