Carl Izzo Consultant

Coating Long Tubes

Question: I'm a manufacturing engineer who was recently hired on to look at paint problems.

Read More

Structural Steel Pretreatment

Question: I am an industrial consultant.

Read More

Panel Preparation

Question: Your answer to P.R. in the January, 2005 Painting Clinic, regarding panel preparation seems, at least to me, incomplete.

Read More

Packaging Freshly Painted Parts

Question: I have worked with the finishing group for my company for more than 10 years now and today I have a question for you.

Read More

Automobile Painting

Question: I hope you can advise or give some direction as to where I could go to get the type of training to become a successful automobile painter.

Read More

Repainting Golf Balls

Question: I have a customer who is looking at a new business of refinishing recovered (salvaged) golf balls.

Read More

Estimating Painting Job Cost

Question I came across your name in the Painting Forum.

Read More

Test Panel Preparation

Question: I am chair of a historical society paint committee which is trying to determine the correct paint colors used by a long-defunct railroad company for their equipment and structures.

Read More

Painting Plastics

Question: Could you provide me with more information on non-metallic coatings on plastics, like plastic coatings on a plastic substrate?

Read More

Stripping Hangers

Question: I use steel angles as part of a racking system to horizontally coat aluminum extrusions with high-performance, high-temperature materials.

Read More

Adhesion of UV-Cured Ink to UV-Cured Coating

Question: I am a printing shop supervisor searching for a UV-cured ink, which can be printed onto a metal substrate that has been powder coated with a polyester paint.

Read More

Using Aluminum at Sea

Quesiton: My company deploys equipment housed in an enclosure that is located in a mild salt-spray environment but no sun/UV exposure.

Read More
PF Podcast
Heatmax Heaters ad with immersion heaters
Metal Pretreatment Technology
Heatmax Heaters ad with immersion heaters
find masking products online
Filtration Systems
Pretreatment Washer and Finishing Equipment
The Finishing Industry’s Education and Networking Resource
Non-Cyanide Silver Plating, AMS 2411J