Cross-Hatch Adhesion Testers Available in Kits
Five kits, three in accordance with ISO 2409 and two in accordance with ASTM D3359.
![PosiTest Kit](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/pf/2024-pf/0424-pf-innovations-bykgardner.jpg;maxWidth=385)
Paul N. Gardner USA’s cross-hatch adhesion testers called PosiTest CH are available in five different kits. Each kit comes with a cross-hatch tool, blade, magnifier (3x (ISO) or 10x (ASTM)), adhesive tape (ISO or ASTM), brush, scissors, 3/32" hex key, ISO/ASTM classification reference chart, instruction manual, hard shell case and a 2-year warranty.
The product determines a coating's ability to resist separation from a substrate when a lattice pattern is cut into the coating in accordance with a specified standard.
The tester conforms to ISO 2409/16276-2, ASTM D3359, AS 3894.9/1580.408.4, JIS K 5600-5-6 and is ideal for coatings up to 250 microns (10 mils) depending on blade and standard.
The kit includes all tools and accessories required for cross-hatch testing; has an ergonomic tool handle with non-slip grip and pivoting cutting head; has a range of easy to replace, high-grade hardened steel 4-in-1 cutting blades; choice of adhesive tape that conforms to ISO 2409 or ASTM D3359.
The illuminated magnifier is available with 3x or 10x. A brush is included to remove any detached flakes from the coating, and a durable hard shell case keeps contents secure.