Solution Removes Metalworking Oils, Inhibits Rust
Kyzen’s Metalnox M6324CP is a heavy-duty alkaline cleaner can remove difficult soils including carbon smut and chlorinated oils.
Kyzen’s Metalnox M6324CP is a heavy-duty alkaline cleaner and inhibitor formulated to remove paraffinic oils used in a range of machining, stamping and deep-draw operations, and provide long-term protection from rust.
The non-flammable, biodegradable aqueous solution can remove difficult soils including carbon smut and chlorinated oils, and provides effective steel corrosion protection for up to 90 days, the company says.
Related Content
-
Corrosion Resistance Testing for Powder Coating
Salt spray can be useful to help compare different pretreatment methods and coatings but it does not tell us much about the corrosion resistance of a part over time in the field. Powder coating expert Rodger Talbert offers insights into how to get a better idea of how to improve a part’s corrosion resistance in the real world.
-
Alkaline Cleaning Guide
Gregg Sanko, Senior Chemist, Oakite Products, Inc. provides an overview of the alkaline cleaning process.
-
TTX Environmental Solves Customer Issue with Electro-Ceramic Desalination Wastewater Processing
Electroplating facility without access to a drainage system found a safe solution for wastewater treatment and reuse.