Anodizing
Blistering of Anodic Coating on 7075 Alloy
We are facing a blister problem on 7075 alloy inside the bore diameter of our cylinder base. We noticed that this problem is occurring during dyeing process and not after hard anodizing.
Read MoreGE picks Alabama for new engine coatings plant
$45 million plant is projected to employ 300 to 400 workers, building components for the F136 jet engine.
Read MoreFlying High with BSAA: Environmentally friendly alternative to chromic acid anodize
BSAA oxide coating exhibits many of the same properties as the aluminum oxide coating that is derived from the chromic acid process.
Read MoreBrazilian coating economy starting to slow
ABRAFATI director says growth to fall form 10% to 4%
Read MoreA Mighty Wind for Finishers
Here in the U.S., the wind energy market grew by about 60 percent from 2009 to 2010, and with more than 40,000 installed megawatts, we rank second to China. Those numbers have caught the attention of finishers, who see a new market to plate parts, e-coat or powder coat turbines, or paint and anodize the hundreds of necessary components.
Read MoreMeasuring the Surface Area of Fasteners
How do you measure the surface area of a threaded fastener? How much coating would you put on it? How thick of a coating? What about non-threaded fasteners? The U.S. Department of Agriculture’s Forest Service, of all people, may have come up with the solution for those pondering how to coat sometimes-difficult small pieces using computer imaging and software to compute the area.
Read MoreProtective Coatings Properties are Topic of Proposed New ASTM Standard
Dry fall coatings are manufactured and sold by a number of coating manufacturers and their inherent dry fall properties are critical in avoiding damage to property adjacent to and below spraying operations, yet there is no known standardized procedure to evaluate whether these coatings possess dry fall properties on surfaces of varying temperature.
Read MoreYou’re Fired
So think back to your first day on the job. Remember the healthy mix of enthusiasm, eagerness and anxiety wrapping around you. You likely had a list—mental or written—of how you could do it better than your predecessor.
Read MoreInvestigation of Tin Whisker Formation
Immersion tin and lead-free hot air solder leveling (HASL) coatings based on SnCu or SnAgCu alloys are widely used as surface finish materials for printed circuit boards (PCB). These coatings prevent the underlying copper from corrosion and preserve its solderability during lead-free assembly processes and for a long storage life of PCBs.
Read More