Ask An Expert: Blistering of Anodic Coating on 7075 Alloy

Q. We are facing a blister problem on 7075 alloy inside the bore diameter of our cylinder base. We noticed that this problem is occurring during dyeing process and not after hard anodizing. Can you please advise us what could be the reason? S.C.

Read More
Anodizing

Hardcoat Anodize Thickness Problem

During the anodizing cycle, how can we check to see if the coating thickness is reaching the thickness requirement stated on the drawing?

Read More
Anodizing

Is it Anodized or Not?

What would be the best way to indicate whether or not an aluminum part has been electro-polished and anodized?

Read More
Anodizing

Technical References for Anodizing

Are there any resources to read and keep on hand as references for troubleshooting appearance issues?

Read More
Parts Cleaning

Just How Clean Is Clean?

Most finishing consultants have lost count of the number of times that inadequate cleaning and pretreatment was the cause of defective painting or plating. Skip plating, blistering, delamination—these are just some of the commonly found defects caused by poor cleaning.

Read More
Anodizing

New Coating Could Mean Cheaper Solar Cells

An MIT website says a novel way to make thin, uniform coatings developed at Rice University could reduce the cost of making conventional silicon solar cells, and could open the way for new kinds of solar cells that are far more efficient or cheaper than conventional ones.

Read More
education

Climbing the Nadcap Ladder for Certification

The Nadcap program is recognized as the premier accreditation program for aerospace and defense contractor supplier accreditation. With this accreditation, an anodizer can effectively access the supplier world of the aerospace and defense industries. We’ll lay out a road map for accreditation that is logical and achievable for someone committed to the excellence required to get to the end goal.

Read More
Liquid Coating

KIRCHNER: 'And you can quote me on that!'

Eight memorable quotes to run your business by.

Read More
Anodizing

Study Says Metal Orthopedic Implants Unlikely to Trigger Allergy

Despite concerns about cobalt and chromium coating debris on metal hip replacements, noted dermatologist says there is little risk that patients will have a skin reaction or joint pain from the devices.

Read More
Anodizing

Sapa Announces $2 Million Expansion of Miami Anodizing Operations

Completion and full operation slated for mid-first quarter, 2012.

Read More
Luster-On Products
Heatmax Heaters ad with immersion heaters
plating and surface finishing additives
Heatmax Heaters ad with immersion heaters
find masking products online
Pretreatment Washer and Finishing Equipment
OptiCenter All-in-One OC11
PF Podcast
cfs masking