Anodizing

Anodizing

Change in Aqueous Cleaning Process

Question: Our use of a non-etch, alkaline soap cleaner has been an old and reliable standby for in-house cleaning of parts that we then send to an outside vendor for additional cleaning and chromating (chem film). Our vendor has decided to change from an alkaline cleaner to an acidic cleaner and this has raised some questions.

Read More
economics

Chem Film Over A Black Anodized Coating

Question: We are working on some parts with the following customer specification: Black hardcoat anodize (Type III, class 2) to match #37038 (FED-STD-595), followed by a Class 3 chromate conversion coating over which we are to apply a primer and black paint to #37038.

Read More
Anodizing

Masking Techniques

Question: We are looking for a better way of masking off areas on a number of machined parts.

Read More
Anodizing

Black Chrome or Nickel

Question: We have a customer that wants to black chrome aluminum motorcycle rims.

Read More
Electrocoating

Lean Six Sigma Enters the Finishing Arena

An exclusive interview with the Juran Institute's President and Chief Executive Officer, Joseph De Feo...

Read More
Anodizing

Alternatives to Prepainted Aluminum

Question: We are a lighting fixture manufacturing company.

Read More
Anodizing

White Spots on Anodized Parts Dyed Black

Question: We are having a problem with very small “white” spots that appear on our parts that we anodize and then dye black.

Read More
Anodizing

Hardcoat Anodizing Controls

Question: We operate a hardcoat anodize tank and we are having trouble getting thicker coatings of 2.0 mils, or slightly greater, without running the loads for more than an hour.

Read More
Anodizing

Laser Engraving Anodized Aluminum

Question: We have an issue with a 30-watt CO2 laser engraver that we are using to mark our aluminum parts.

Read More
Electroplating

Expecting The Unexpected

When Murphy's Law "unexpectedly" delivered five critical parts for simultaneous finishing, instead of the usual one or two, they were processed quickly and without breaking a sweat. Explanation—this supply chain had planned for contingencies everyone agreed would "probably" never materialize...

Read More
Luster-On Products
PF Podcast
Products Finishing Top Shops Benchmarking Survey
Metal Pretreatment Technology
Filtration Systems
Products Finishing 40 Under 40
PMTS 2025 Register Now!
Mocap Masking Caps Plugs Tapes
Products Finishing 40 Under 40