Painting Stainless Steel
We are concerned about paint adhesion on equipment cabinets made of mostly 41003 (a utility-grade stainless steel that is 12 percent Cr) and either 304 or 201 for the hard-to-draw parts.
Read MoreStirred, Not Shaken
My group has responsibility for process specification BAC5736 regarding mixing of an epoxy primer. Here is my interpretation of the specification.
Read MoreAkzoNobel Powder Coatings Receives Innovation Award
Haworth 2011 Supplier Innovation Award for developing its Interpon F2010 furniture product/technology
Read MoreFungus-Resistant Topcoat
We are using a mil spec polyurethane topcoat, MIL-PRF-85285, on an electronics housing, and I am trying to find a reference indicating that this topcoat is fungus-resistant.
Read MorePowder Coating Training Class is Aug. 14-15
Parker Ionics hosts PCI training course in Westland, Michigan
Read MoreSIFCO ASC Featured on FOX Business Network
“Manufacturing Marvels” segment on The Willis Report on FOX Business Network. The episode airs Friday, July 27 from 9:00-10:00pm EST.
Read MoreDrying Gold-Plated Parts
What is the optimum temperature for drying gold-plated parts? Is there a point where the temperature may become detrimental to the gold-plated surface?
Read MoreFinish Brightness
Finished lots of parts ostensibly with the same plated finish “look” very different each time they are received. Is there a more trustworthy process to determine the brightness of the finished part?
Read MoreBurnt Nickel
I am having a problem with burning on my nickel-plated parts. On some jobs, 75 to 85 percent of the parts come out with burnt areas. Do you have any suggestions as to what the cause of this might be?