Liquid Coating
Swirl Marks In The Paint
We have a rather large plastic part. After painting it shows swirls that appear to be made by a brush. swirls are positive and can be felt using one’s finger. Can you make any suggestions as to what might be causing this problem? Could there be a residue from the wash left on the surface or something in the molding of the part?
Read MoreProductive Plastic Painting
Upgrades improve paint system flexibility, application characteristics
Read MoreTraining Classes
Do you teach any paint or industrial coating classes? If not, do you happen to know where I could find one?
Read MoreWrinkle Finish
I am painting a machine tool sheet metal cover and having a hard time finding someone who can apply a wrinkle finish.
Read MoreStainless Steel Smokestack
I want to replace the mild steel smoke stack on the steam boiler with one made from stainless steel. The new smokestack material is 3 mm thick. What treatment do you recommend I apply to keep the paint from peeling off?
Read MoreAdhesion to Stainless Steel
We have made some process improvements over the last year but are still plagued with paint peeling from the kick panels. We have in the past seen a silicone contamination issue and it did cause some fish-eye problems in our aluminum painting process, but nothing that affected adhesion. Do you have any suggestions as to what the cause might be? Anything new to the industry that we should investigate? We are looking for longer-term adhesion.
Read MoreBLISTERING USING AIRLESS SPRAY
The logical approach would be to slow down the solvent balance a bit to assure flow, but with airless you have to be careful not to sag. Do you think that this is a plausible explanation for the blisters?
Read MoreZINC-RICH PRIMER
One customer wants to use a zinc-rich primer and TGIC-free top coat. After applying both the coats the painted test panels are failing mechanical properties. How can we resolve this issue?
Read MoreFARADAY CAGE EFFECT
What I don’t know is if holes, penetrations completely through the material, are also a problem? Should I be concerned for lack of DFT (dry film thickness) on the surfaces inside the holes due to FCE or since these are “holes” and not recesses, would I be OK pursuing this coating process?
Read MorePAINTING GALVANIZED TANK
I have a 750–1000 gal galvanized holding tank used for maple syrup production. I would like to remove the rust and coat the inside of the tank. Because of the use and need for it to be food safe I am unsure of what to use to coat/paint it. Any ideas? Also, if you have another recommended paint application method besides electrostatic, I’d be willing to entertain that too.