sales
Painting Viscosity vs. Temperature
One reader has something to add about paint temperature to Carl's response in the December 2012 column regarding spraying high-viscosity paints.
Read MorePlating Q&A: Low Stress Nickel Deposit
Plating expert Art Kushner answers a question about parts that specify a “low stress” nickel deposit, and whether there are numerical ranges for high- and low- stress nickel deposits.
Read MorePainting Particle Board
I am looking for a paint or coating that can be used to coat the surface of the particle board panels in a production line environment after finish sanding and prior to a paper laminating process.
Read MoreFingerprints on Plated Parts
I have received two questions in the last few months regarding fingerprints on finished plated parts. This is not an uncommon problem in the world of plating. Looking through my archives, I realized it would be good to revisit this topic:
Read MoreCuring Polyurethane on Wood
Can you help us find a polyurethane varnish that will cure in our warm-air oven?
Read MorePaint Stripping Waste Disposal
In response to a question in the September 2012 column regarding the disposal of waste from paint stripping, one reader recommends purchase of a stripping oven, used to strip products and paint racks.
Read MorePowder Coat Q&A: A Good System Gone Bad
Rodger Tallbert answers a question about a problem with light coating on an automotive product, where the coater is not getting the kind of coverage they got when the system was new.
Read MorePitted and Rough Nickel Plate
How can I remove roughness and pitting in my Watts nickel plating bath?
Read MoreOn-Site Treatment or Off-Site Disposal
Can you provide information on a pH/precipitation system that will speed up the process of removing metals and patina chemicals from wastewater?