sales
Metallic Powder Coating
Do I need to clear coat the entire wheel? Do you typically clear coat over metallic powder coat? Are there any advantages or disadvantages?
Read MoreReactive Waste or Not
It is very, very difficult for us to accept that this waste is “reactive.” Do you have any advice?
Read MoreLevel Nickel
The problem that we observed is poor leveling and the inability to cover minor defects on the surface.
Read MorePaint Color Shift
We recently noticed our paint use was increasing, so we checked the dump tank and found it full of paint because the discharge valve was leaking. Now we are having trouble with color shifting and hiding of the painted parts.
Read MorePaint Filter Disposal
I am confused about how to properly dispose of filters from a recently installed paint booth.
Read MoreMix-Up 101
One of our operators used nitric acid to adjust the pH of our nickel plating solution. Is there any way that we can salvage this solution or do we have to dump the tank and make up a new tank?
Read MorePainting Polystyrene Insulation
We ended up covering the lagging with sheet metal, which we painted with our standard paint finish to match our units. I am looking for a less expensive way to lag our air tanks. Do you have any good ideas?
Read MoreRinsing Problems Again
We triple rinse our parts after our final decorative chromium plating step. However even with this type of rinsing, we end up with spotted parts after drying.
Read MorePaint Shop Life Cycle Management
Proper planning can help make your paint operations productive from cradle to grave
Read More