Electrocleaning in a Barrel
Can you perform electrocleaning in a plating barrel?
Q. Can you perform electrocleaning in a plating barrel? C.A.
A. Yes, you can perform both anodic and cathodic electrocleaning in a barrel. The following link gives a brief overview of the electrocleaning process used in the plating industry: pfonline.com/articles/preparation-for-electroplating. This article is a concise overview of types of soils that can be removed using the process. It also describes different types of cleaners and contains a number of illustrations that you can review.
Related Content
-
Pretreatment of Black Oxide
Having issues achieving a consistent color with the application of black oxide? Start by looking at your pretreatment. Connor Callais of Hubbard-Hall offers advice for troubleshooting your black oxide process.
-
Corrosion Resistance Testing for Powder Coating
Salt spray can be useful to help compare different pretreatment methods and coatings but it does not tell us much about the corrosion resistance of a part over time in the field. Powder coating expert Rodger Talbert offers insights into how to get a better idea of how to improve a part’s corrosion resistance in the real world.
-
Clean Technology Lasers for Coating Adhesion
Laser cleaning systems remove corrosion, grease, residue and existing coatings from metal surfaces quickly, with less preparation and mess than traditional techniques.