![powder coating](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/PF/2022-PF/1222pfphotofinish3.jpg;maxWidth=720)
A&A Powder Coatings (Hunt Valley, Md.) has served the Maryland, Pennsylvania, and Virginia areas for 30 years, providing powder coating needs to a range of industries including the industrial, medical, hospitality, military, electrical, fencing and automotive sectors. With a 575-foot conveyor system, A&A is always looking to expand its field of clients, offering quick turn-around, quality products, customer communication, a range of masking, and safe packaging.
![powder coating](https://d2n4wb9orp1vta.cloudfront.net/cms/brand/PF/2022-PF/1222pfphotofinish.jpg;maxWidth=385)
A&A’s powder system features an iron-phosphate wash to ensure proper pre-treatment, 8 automatic oscillating guns, batch booth and cure oven, as well as a burn off oven. Trained coaters ensure proper coverage of parts and are ready for any request.
Related Content
-
Adjusting Current and Voltage When Powder Coating
Which manual powder coating gun setting is better to adjust, voltage or current? Jeff Hale of Gema USA discusses when to use different settings on your powder gun to achieve optimal results.
-
Touch-up Options for Powder Coated Parts
Is it true that powder coating cannot be touched up? Powder coating expert Rodger Talbert offers options for powder coating touch-ups.
-
Conveyors and Paint Systems
Choosing the right conveyor system, coating technology, and ancillary equipment.