Tops Shops Profile: Tanury Industries
Tanury Industries offers plating and PVD finishes for the jewelry, aerospace and architectural industries. The company says it is the largest jewelry plater in the U.S.
About: Tanury Industries offers plating and PVD finishes for the jewelry, aerospace and architectural industries. The company says it is the largest jewelry plater in the U.S.
Location: Lincoln, Rhode Island.
Top Officials: Thomas Tanury, Chairman; Michael Akkaoui, President and CEO.
History: Founded in 1946 by the Tanury family, the firm grew quickly from a 7,200 square-foot facility into an operational footprint of over 70,000 square feet and has become the leading finisher for the jewelry industry.
Related Content
-
Hexavalent-Chromium-Free Aluminum Sacrificial Paint Validation
Hexavalent chromium is a known carcinogen, repro-toxin and mutagen. Its elimination is of high importance to the aerospace industry, which has struggled to find high performing alternatives. Legacy aluminum sacrificial paints have traditionally utilized hexavalent chromium to prevent corrosion and coatings which are equal to or better than have been difficult. This second of two papers discusses the hexavalent-chromium-free process from the user point-of-view in terms of the process validation work by Rolls Royce Corporation.
-
Anodizing for Bonding Applications in Aerospace
Anodizing for pre-prep bonding bridges the gap between metallic and composite worlds, as it provides a superior surface in many applications on aluminum components for bonding to these composites.
-
The Solution to Costly Aircraft Paint Adhesion Failure
Lucas Dillingham, of surface inspection technology provider Brighton Science, offers insights for avoiding aircraft paint defects and adhesion failures.