That Sticky Feeling

Question: We operate a Type III (hard anodize) bath which operates at the following conditions: 15% sulfuric plus 1% oxalic, dissolved aluminum less than 7.5 g/l, 40F, aluminum cathodes, air agitation, solution is filtered.

Read More
Anodizing

"Bleach Test" Feedback

I was surprised at the interest in the so-called "Bleach Test" that I wrote about in the February issue.

Read More

Chromate Conversion Coatings

  Question It seems to be a widely known fact that you are not supposed to expose chromate conversion coating on aluminum to temperatures greater than 160F because the coating will deteriorate.

Read More
Anodizing

"Bleach Test" for Quality of Anodic Seal

Question: A customer of ours has asked us to conduct a bleach test on its parts that have been sulfuric acid anodized, dyed and sealed.

Read More

Smut and Desmutting

Question: I am new to this industry and have heard about smut and desmutting operations.

Read More
Parts Cleaning

Pretreatment of Aluminum for Powder Coating

Question: What is the best way of treating aluminum before powder coating?

Read More
Electroplating

Vacuum Deposition of Selenium

Question: We vacuum deposit selenium on 3003 and 6063 aluminum alloy drums for copy machines.

Read More
Anodizing

Stripping Anodic Coating

Question: What is the best way to strip an anodize coating?

Read More
Anodizing

Anodic Coating Blisters on 7075

Question: We do Type III (hardcoat) anodizing.

Read More
Electroplating

Dual Purpose Anodizing Bath

Question: When using a sulfuric acid-oxalic acid electrolyte for Type III hardcoat, is it possible to raise the temperature in order to do Type II anodizing in the same tank?

Read More
Metal Pretreatment Technology
Mocap Masking Caps Plugs Tapes
Pretreatment Washer and Finishing Equipment
PMTS 2025 Register Now!
find masking products online
Products Finishing Top Shops Benchmarking Survey
Filtration Systems
The Finishing Industry’s Education and Networking Resource
Products Finishing Top Shops Benchmarking Survey