Products
Silicone Pull Plugs Mask Threaded, Non-Threaded Through Holes
Caplugs’ SPP-SH Series pull plugs are made from durable silicone, are reusable and can withstand temperatures as high as 600°F (315°C).
Read MoreEmergency Decontamination Booths Come Fully Assembled
Hemco Corp.’s emergency shower booths are molded from one-piece, seamless, chemical-resistant fiberglass and are equipped with a pull-rod-activated shower and push-handle eye/face wash for immediately drenching of personnel that have been exposed to hazardous chemicals.
Read MoreFlexible Topcoat Allows for Maximum Bend without Cracking
Axalta’s Imron 3.5 + FX Flexible Topcoat also provides superior weathering performance, distinctness of image (DOI) and a consistent high-gloss finish to industrial applications.
Read MoreNo-Drip Atomizing Nozzles Eliminate Waste, Finish Problems
Exair’s 1/8 NPT No Drip external-mix atomizing spray nozzles mix liquid and air outside the nozzle and allow the air and liquid flows to be adjusted independently, and offer the added benefit of positively stopping liquid flow when compressed air is shut off.
Read MoreSteel-Belt Tumble Blaster Batch-Processes Parts in a Single Cycle
Viking Blast & Wash Systems’ Model 1400S industrial tumble blaster is a batch-style cleaning system specifically designed for the high-speed processing of parts that can be gently tumbled.
Read MoreBranch Fusing Enclosures Customized for Specific Heater/Control Combinations
Process Technology says its customized branch fusing enclosures ensure that heater/control circuitry is protected according to normal code requirements.
Read MoreDry Filter Paint Booth Line Includes 500+ Pre-Engineered Models
Global Finishing Solutions’ Dry Filter Paint Booth line includes bench, open-face and enclosed booths suited for a variety of finishing applications. The company has pre-engineered more than 500 models of the booths in sizes ranging from 3- to 20-ft. wide.
Read MorePaint Booths Enable High-Quality Finishes on Medium-Sized Equipment
General Purpose paint booths from Global Finishing Solutions feature strategically placed light fixtures with four-tube fluorescent bulbs, allowing for optimal brightness and color matching.
Read MoreMaterial-Handling System Wirelessly Instructs Movements
Therma-Tron-X’s Automated Conveyor Carrier (ACC) material-handling systems incorporates a wireless network to send instructions to carriers throughout a paint line, providing point-to-point movement for parts ranging from small to heavy.
Read MoreGeorge Koch and Divisions Offer Variety of Surface Finishing Systems
George Koch Sons, along with divisions PriceWalgren and Jessup Systems, designs, manufactures and installs custom surface finishing equipment for applications including electrocoat, liquid/powder paint, plating, phosphate, anodizing and porcelain enamel.
Read MorePowder Coating System Fits Small Footprint, Retains Flexibility
At less than 9,000 ft.2,IntelliFinishing’s Pathfinder base powder coating system still includes multiple load and unload stations, a three-stage wash, a multi-lane cure oven, and complete automation.
Read MoreZinc Phosphating Process Designed to be High Performing, Environmentally Friendly
Hubbard-Hall and Phosfan LLC’s new Phosfan zinc phosphating technology is said to discharge no water, operate at room temperature and produce less sludge—all while also producing a coating with high adhesion and corrosion properties.
Read More