Electroplating
eeling Gold Revisited
Our plating shop is having problems with plating gold components that have been nickel plated. We find that we get inconsistent results with the gold adhering to the nickel plate. This causes peeling and blistering of the gold plate.
Read MoreAging of Plugs
We use nylon, silicone and Teflon masking plugs and screws for electroless nickel on aluminum. Can you tell me what we can expect for aging?
Read MorePlating Electrolytic Nickel on EN
We have adhesion problems when plating nickel over electroless nickel. The bath analysis for both solutions is within the required tolerances. We are not using a nickel strike prior to the electrolytic nickel plating step. Do you have any suggestions?
Read MoreNickel Balls
We have a problem with our EN (high-P): after two to three turnovers, we have nickel balls (about 50-100 microns) forming on our parts; after one to two more turnovers it’s OK again.
Read MoreBrazilian coating economy starting to slow
ABRAFATI director says growth to fall form 10% to 4%
Read MoreGlobal Finishing Solutions announces $10 million expansion
Osseo, Wisconsin corporate offices will grow
Read MoreA Mighty Wind for Finishers
Here in the U.S., the wind energy market grew by about 60 percent from 2009 to 2010, and with more than 40,000 installed megawatts, we rank second to China. Those numbers have caught the attention of finishers, who see a new market to plate parts, e-coat or powder coat turbines, or paint and anodize the hundreds of necessary components.
Read More