Liquid Coating
White Polyester Melting Disk
I am curious if you know of a prefabricated low-temp melting polyester disk (1.5-inch diameter or so) that I could lay down on the top of the hot disk to bond to the clear polyester to create the nice plastic backing.
Read MoreCast Iron Painting Problem
The products are standing bathtubs. The inside is covered with porcelain enamel and the outside is painted. Upon receipt, the customer found all of them to have paint problems—many bubbles formed under the paint layer.
Read MorePainting Galvanized Steel
One of our customers ordered enclosures made of galvanized steel for a special job. I am not sure how to pretreat this material, although I have had many suggestions.
Read MoreLoss of Gloss Over Aluminum Bonnets
I am the paint line manager of a company situated in the Middle East. The temperature here gets up to 55°C (131°F). We paint parts for motor vehicles. We have a problem with loss of gloss on painted parts. Why do we encounter this problem of loss of gloss when using waterborne basecoat system on aluminum bonnets?
Read MoreFish Eye Clear Coat
We’re having a problem with our clear coat. Our base coat paint turns out okay but when we started to clear coat, there came the fish eyes. I was taught that if silicone has been used in or around where you were painting this would happen. How can we correct this problem?
Read MoreSmall Particles, Big Benefits
Combining 100% solids UV-curable coatings with nanotechnology can result in substantial cost savings and other advantages
Read MoreAutomobile Painting Classes
There is an institute (Name Withheld) that will teach painting, custom painting, etc, but you must also sign up for their auto collision and refinishing course. Unfortunately, I learned that these courses would cost me $28,000 as quoted to me by the institute representative. I thought that was FAR too high, and will pursue your advised method of practicing and learning by trial and error, picking up pointers from people I meet, or technical books you can buy at the painter supply shops.
Read MoreDip Tank Equipment
My company is purchasing machined and painted lifting hooks from a third party manufacturer and wish to move these processes in-house. The dipping process seems to work well but I am having a hard time finding a company that makes this type of small-part, low-volume equipment. Do you have any suggestions?
Read MoreBleeding-Out Issue
There is a copper band on the outside circumference on the part which does not require painting so it is covered during paint process. We see very slight bleed-out from under this band after 2–3 days.
Read MoreAutomatic Painting
Our inquiry is about whether we should install an automatic spray coating system for applying a shop primer in our structural steel fabrication facility. This system needs to be able to coat sheet metal and structural profiles in different shapes like I, U and so on. Is automatic coating a satisfactory method to paint these parts or shall we coat them manually?
Read More