Powder Coating
Splotchy Appearance in Coating
We use manual spray guns to apply a textured powder over a cast part, and that black finishes have a dark/light, splotchy look to them after they are cured.How can wer get better appearance?
Read MoreBubbles in Steel
We apply powder coating over steel parts that have been treated with a zinc phosphate. Some parts show bubbling after running through the powder line. The parts were clean and rust-free before running. What could cause a bubble/blister on steel parts?
Read MoreYellow Tint to Parts
Some parts have a slightly yellow tint to them after running through out two-stage zinc phosphate line, even when we lower the free iron. Do you have any ideas what this could be?
Read MoreCCAI SoCal Chapter Partners with Marines on 'Toys for Tots' Event
Nearly 190 toys collected to help disadvantaged kids
Read MoreReducing Cure Time with a Hybrid Oven
Is it possible to decrease the curing time to fewer than 9 min if we change the oven to a hybrid system with combined infrared (IR) and convection heating?
Read MorePPG Also Wins $1.5 Million Through DoD’s SERDP
PPG will work with ARL to develop a powder topcoat that will meet military standards for ultraviolet durability, matte finish and resistance to chemical agents.
Read MoreImpact of REACH Regulation on the Global Finishing Market
This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2012 in Las Vegas, Nev., on June 12, 2012.
Read MorePowder Coating's Future
There for a time, powder coating shops were popping up on every corner. Now it seems everyone has figured out that margins are extremely tight and that powder coating is not as easy as the guys who sell it might like for you to believe. What do you think the future holds for powder coaters?
Read MoreQuestions and Answers for Pretreatment Options
Are you aware of any uncomplicated, user-friendly pretreatments that are compatible with powder coating, will inhibit rust on surfaces with deep inset corrosion and will accelerate beneath the coating after the process is complete?
Read More