sales
Zinc Contamination
How do we remove zinc from our nickel tanks after copper/nickel/chromium plating?
Read MoreCoating Analysis
What are the most energy-intensive areas one can intervene in a standard coating process?
Read MoreDisappearing Brass
Why does the brass seem to disappear on brass-plated zinc castings after we lacquer and bake the parts?
Read MoreLow-Temperature Zinc Phosphate
Can you give me any advice on lower-temperature zinc phosphate pretreatment products I can use before powder coating steel?
Read MoreNASF Launches Comprehensive Surface Finishing Guide
"Advanced Surface Technology" is one of the most comprehensive reference to date for a wide range of coating and finishing applications, as the publication is both a practical guide for any professional or operation in the coatings value chain.
Read MoreBurnt Plating Deposits
Can you give me a better understanding of the phenomenon of "burnt" deposits on cathodes?
Read MoreTrojan Powder Coating Paints Modern Valentine for New York City
Match-Maker, a unique installation designed to connect perfect strangers, was selected by the Times Square Alliance and the Van Alen Institute as the featured design for this year’s Valentine’s Day heart.
Read MoreCCAI SoCal Golf Outing Brings In 289 Toys For Tots
Joined by eight Marines, this second annual event beat last year’s outing by bringing in close to 100 more toys and nearly doubling the amount of golfers to a sold out 76. See The Video!
Watch