sales
Rinsing Blind Holes Prior to Dying
I have problems with leaching from blind holes in black anodized parts.
Read MoreMirror Chrome Finish
n the process used to achieve the chrome plate specified in ASTM B456, do you polish the parts before or after the electrodeposited coating?
Read MoreNew Jersey Lt. Gov. Visits Metal Finishing Company
Financial assistance from NJ allows Superior Powder Coating to add 16 more workers to the 139 current employees.
Read MorePhosphating Dust and Overspray
How can we cut phosphating dust after zinc phosphate and passivating stages, and reduce overspray losses in our water wash spray booth?
Read MoreNASF Board of Directors Recognize Four Departing Members
Pat Gleason, Ray Lucas, Bill Wiggins and Joelie Zak leaving NASF Board
Read MoreFinding Paint Testing Laboratories
We occasionally have problems with insufficient paint adhesion. Where would I find a lab to perform an in-depth analysis of the adhesion among the interface of our paint, a base coat and primer material?
Read MoreFloating Floc Causing Issues
We are a contract finisher with anodizing, alkaline zinc plating, electrocoat and powder coat capabilities. Our processes are well-established, but a few days ago we suddenly experienced floc rising, rather than settling, in our waste treatment. What I should check?
Read MoreAnodizing: Current Density vs. Voltage
Can you detail the procedure for anodizing using the current density method? What are the quality advantages for us to completely change our processing technique?
Read MoreNASF and Southern California Metal Finishers Kick Off Bright Design Challenge
Students are challenged to create innovative works utilizing plating technologies; top three concepts as judged by the panel be awarded $5,000 scholarships.
Read MorePPG Aerospace Special-Effect Coatings Bring Virgin Atlantic Airways’ Livery To Life
Proprietary PPG pigment gives highly-reflective, vibrant color to airline’s vision
Read More