sales
Blistering of Anodic Coating on 7075 Alloy
We are facing a blister problem on 7075 alloy inside the bore diameter of our cylinder base. We noticed that this problem is occurring during dyeing process and not after hard anodizing.
Read MoreWhere is the Pipe Glue?
I have contacted several plumbing suppliers around me, and none of them were able to assist me in finding the glue that you recommended for CPVC pipe or the pipe tape. We are seeing exactly what you were talking about on leaky pipe containing caustic or alkaline solutions and would love to put them to rest.
Read MorePinholes in Powder
We have a problem with a concentration of fine, dense pinholes in our powder film. The coating is a urethane-polyester that is applied over a part that has been electro-coated. The substrate is sheet metal. The problem is much worse when the powder film is heavier.
Read MoreMetal Preparation of Steel
We are planning to powder coat the part with a TGIC polyester, but we do not have a system yet. Will it be acceptable to blast the surface and not add any chemical pretreatment? Do I need a primer coat under the TGIC polyester?
Read MoreTraining Programs
Where can I get some information about training programs for electroplaters?
Read MoreMagnetic Parts
I am having problems with parts that are magnetic. Can you give me any information concerning magnetized steel and the effect on plating adhesion?
Read MoreDecoding Process Abbreviations
Some of the information that comes with the jewelry products we import from Spain states that they are coated with a gold IPG material. Why use an IPG coating?
Read MoreTrivalent Chromium Reduction
I am trying to reduce the trivalent chrome in a hexavalent chrome tank.
Read More