A Conversation With ... Scott Pavlish, Pavco Inc.
Scott Pavlish wasn’t around when his family started Pavco Inc. back in 1948, but his leadership of the company in the last decade has been just as important. Pavlish is president of one of the leading developers of chemical processes in the metal finishing industry.
Read MoreChloride Concentrations
Can you give me a titration procedure to check chloride concentrations in the PC-667 acid copper bath?
Read MoreGuys Like Ray Lucas Make A Shining Example
Having the U.S. Environmental Protection Agency show up at your front door on a Monday morning is never a good sign—kind of like Mike Wallace and a 60 Minutes crew, or maybe even your in-laws. But Ray Lucas and his employees at Valley Chrome Plating in Clovis, Calif., just didn’t see it that way.
Read MorePositive Energy Growth
Chrome Deposit Corp. reduces its energy use, minimizes its environmental impact and improves its energy-management practices.
Read MoreRipple Effect: Researchers say leveling of electrodeposits can be achieved by applying a small forcing voltage
Seeking smoother plating deposits? It may be all in the waves. This story looks at studies that have shown that superimposition of a small sinusoidal potential wave (smooth, repetitive oscillation) onto a potentiostatic bias can lead to more level electrodeposits in finishing.
Read MorePlating on Tellurium Copper Alloys Plating on Tellurium Copper Alloys
I cannot achieve uniform adhesion of either Wood’s nickel or cyanide copper on C14500, tellurium-bearing copper. I clean using reverse current followed by 11 percent HCl, a Wood’s nickel strike and a silver strike. After stripping the failed plate and repeating the process, I sometimes have much better adhesion. Is this due to the aggressive etch provided by the stripping process or better oxide removal provided by the process?
Read MoreMore on Magnetic Parts
In the November 2011 issue of Products Finishing I briefly discussed problems with plating magnetic parts. One of my readers (also a student of mine some 25 years ago) sent me an email mentioning some other causes of parts becoming magnetic. One has to do with the machining and preparation of the parts.
Read MoreNASF Connecticut Chapter Holding Supplier Exhibition March 6
All proceeds at the event are used to sponsor the Connecticut Branch’s College Scholarship, which is given to a child of a Connecticut Branch member.
Read MoreElectronic Precision Specialties Wins 'Metal Finishing Model Shop Award'
The California/EPA Department of Toxic Substances and Control has recognized Electronic Precision Specialties, Inc., with the "Metal Finishing Model Shop Award," only the fourth shop to receive the award.
Read More