Electroplating

Copper In My Chromium Tank

Question: How can I remove copper from my chromium-plating tank?

Read More

Electrolytic Nickel Plating On Aluminum

Question: Can you suggest a process for plating electrolytic nickel on zincated aluminum?

Read More

Chromium Plating and Recessed Areas

Question: How can we improve the coverage of our chromium plating in recessed areas?

Read More

Replacing Copper Cyanide Strike Baths

Question: We use a copper cyanide strike bath and would like to replace it with a non-cyanide type bath.

Read More

Low Stress Nickel Deposit

Question: We receive parts that specify a “low stress” nickel deposit.

Read More

Low-Nickel Seal is Modern Solution

This mid-temperature low-nickel seal helped Modern Aluminum Finishing solve a number of problems...  

Read More

Whitewash

Question: Recently, we had to perform a brightener conversion on our bright nickel process as the supplier discontinued one of the brightener components.

Read More

Zinc Treatment

Question: Your March 2003, article, “Increased Floc,” prompted me to write regarding a similar problem we just started having.

Read More

More Floc

Question: Steve, in your March 2003 “Increased Floc” article, you responded to a reader’s question regarding increasing amount of floc in the wastewater pretreatment clarifier even though “nothing in our operations or chemistries has changed...” Chances are that something did indeed change, and detective work is needed to find the culprit.

Read More

Chem Film Staining

Question: I operate a clear and yellow chromating (chem film) Irridite line.

Read More
Rectifiers for the Plating Industry
Hitachi High-Tech FT200 series
TriMac BLUE™
KCH Engineered Systems
Luster-On Products
In-Place Repairs for Canning Presses
Koch Finishing Systems
Pretreatment Washer and Finishing Equipment
TriMac BLUE™