marketing
A Look at Early Advertising in the Surface Finishing Industry
This article contains a collection of the advertisements published in the July, 1930 issue of Metal Cleaning and Finishing. They capture an instant in time, when the surface finishing industry was quite different from what we find today.
Read MoreDevelopment of Life Prediction Models for High Strength Steel in a Hydrogen Emitting Environment
Solvent substitution for maintenance and overhaul operations of military systems has been a primary environmental concern for many years. Cadmium replacement in these systems has been targeted for decades. Both of these areas have a common obstacle for implementation of any potential alternate. Hydrogen embrittlement of high strength steel is the most predominant unforeseen hurdle since high strength materials show sensitivity to the phenomena and the source of the hydrogen can be anything within the fabrication process, maintenance practice or the natural corrosion cycle. Standardized testing on this issue has traditionally stemmed from the aerospace industry where it is a principal focus.
Read MoreDissolving Titanium Anode Baskets
Has anyone experienced titanium anode baskets dissolving in a nickel sulfamate plating bath with a pH of 2.5 and no current flowing?
Read MoreYellow Tint to Parts
Some parts have a slightly yellow tint to them after running through out two-stage zinc phosphate line, even when we lower the free iron. Do you have any ideas what this could be?
Read MoreHaviland Announces 100% Employee Ownership
Prior to this sale, Haviland Enterprises was owned 54 percent by the Haviland family and 46 percent by Haviland employees.
Read MoreCoating PVC Products
My company manufactures a line of products fabricated from black PVC irrigation pipe, and I would like to be able to offer these products in colors other than black. The coating must be abrasion-resistant enough to withstand metal and plastic objects sliding across its surface without scratching.
Read MoreCCAI SoCal Chapter Partners with Marines on 'Toys for Tots' Event
Nearly 190 toys collected to help disadvantaged kids
Read MorePink Coating on BSA Parts
I understand that iron and poor current can cause a pink coating on boric-sulfuric anodized (BSA) parts. What levels of iron are permissible before reaching the pink-colored coating? Are there any other things we could be missing?
Read MoreReducing Cure Time with a Hybrid Oven
Is it possible to decrease the curing time to fewer than 9 min if we change the oven to a hybrid system with combined infrared (IR) and convection heating?
Read More