Powder Coating
Aluminum Sand Casting Preparation
Question: We have been asked to quote chromate conversion coating for an aluminum sand casting prior to powder coating.
Read MoreSelecting SCR Power Controllers
While it is more geared to the manufacturer of SCR controllers, this article can give finishers some good tips on what to look for when purchasing or building their own SCR power controller…
Read MorePowder Coating and Plating
Question: Although I too write for Products Finishing (Pollution Control Clinic), I am writing you on behalf of one of my clients.
Read MorePreventing Cross Contamination
Since it might spray multiple colors per day, Rapistan must keep stray powder particles from contaminating new colors...
Read MoreEliminating Tooling Marks
Question: A while back you answered a question about special tooling used to form parts that already have a powder coating on them.
Read MoreUpgrading Powder Coating Line
Question: We are a manufacturing company that has been powder coating for about 7 years.
Read MorePreparing Brazed Metal
Question: We manufacture aluminum heat exchangers and are planning to implement CAB brazing soon.
Read MoreConditions for Teflon Coating
Question: I was viewing PF ONLINE and had a question about the conditions for Teflon coating using electrostatic powder coating guns.
Read MoreHerman Miller Adds Powder Coating
The addition of a powder coating line has allowed furniture manufacturer Herman Miller to create interesting and unusual shapes for its state-of-the-art workstations…