additive-manufacturing

3D Printing Part Finishing

How do we finish rough 3D-printed systems?

Read More
Parts Cleaning

Fish Eye Additives

We have been experiencing craters or dimples in our current coating application process. We have spoken with our coating supplier, which said we may need to add an additive to eliminate this. What is this product, and how does it work?

Read More

Additives to Address Contaminant Issues

I have heard that a fish-eye-type additive can be added to the coating to help eliminate what looks like Swiss cheese in my coating after it has been sprayed. Can you give me any insights on this issue?

Read More
Parts Cleaning

Powder on Galvaneal

We have customers that want a smooth powder coating on a galvaneal finish. We prep with a light alcohol wipe, prebake the parts to allow for off-gassing, then spray with a smooth powder. We are having problems with “craters” and specs, so the surfaces won’t pass a class “A” test. Is there a way to coat a galvaneal part with a smooth powder that does not have a special additive?

Read More

Ionic Liquid [BMPy]Br as an Effective Additive During Zinc Electrodeposition from an Aqueous Sulfate Bath

The effects of a new ionic liquid additive 1-butyl-3-methylpyridinium bromide [BMPy]Br on the electrodeposition of zinc on steel substrates from acidic sulfate solution was investigated by employing potentiodynamic polarization and cyclic voltammetry techniques complemented with XRD and SEM measurements.

Read More
Anodizing

Improvement of Corrosion Resistance of Magnesium by Anodizing in Alkaline Electrolytes

Results show that the novel organic additive reduced the sparking voltage and provided a relatively smoother surface.

Read More
Powder Coating

Powder Coating Plastics

Is there a specific additive that can be added to an injection molded ABS plastic part to allow it to accept a powder coating?

Read More

Back to the Old Grind Again

Question: In the November 2003 issue of the Painting Clinic (www.pfonline.com/articles/clinics/1103cl_paint5.html), you replied to B.B. regarding the addition of a heat insulating additive to his paint material.

Read More

Back to the Old Grind

Question: Sir, I have purchased a granular powder that is a heat resistant additive and has to be added into the paint as 20% addition.

Read More
Pretreatment Washer and Finishing Equipment
Filtration Systems
New Acid-Free Bright Nickel Process
plating and surface finishing additives
find masking products online
OptiCenter All-in-One OC11
Heatmax Heaters ad with immersion heaters
The Finishing Industry’s Education and Networking Resource
Non-Cyanide Silver Plating, AMS 2411J