surfin
Zinc Alloy Process Provides Ductile Deposits, Faster Plate Times
At Sur/Fin 2018, Haviland Products Co. will feature its Havalloy ZN-TCP zinc-nickel alloy plating process, designed to provide ductile deposits and faster plate times on complex-shaped parts containing 13-15 percent nickel by weight.
Read MoreSoftware Apps Replace Paper-Based Recording
At Sur/Fin 2018, Anoplex Software will showcase tablet-based JobPro and ChemTrak options for job tracking, job data collection, and chemical process control, designed to replace routers, add-sheets, makeup sheets, temperature logs, and other paper records.
Read MoreAlkaline Zinc Systems Reduce Rejects, Increase Productivity
Asterion will showcase its RoHS-compliant Asterion Ultra alkaline zinc systems at Sur/Fin 2018, designed to provide corrosion protection while reducing rejects, increasing productivity and enhancing appearance.
Read MoreElectroplating Method Suited for Small Components
Technic will showcase a variety of technologies for industrial and electronic finishing at Sur/Fin 2018, including its Spouted Bed Electrode (SBE), a patented method of electroplating small components such as electronic connectors, pins, chip capacitors and resistors.
Read MoreDevices Offer Diagnostics for Improved pH/ORP Monitoring, Control
GF Piping Systems will feature Signet 2751 DryLoc pH/ORP Smart Sensor Electronics at Sur/Fin 2018, designed for probe health, glass impedance and broken glass detection for improved pH/oxidation-reduction potential (ORP) monitoring and control.
Read MoreRoom-Temp Anodic Seals Outperform Hot Dichromate Seals
At Sur/Fin 2018, Chemeon will highlight the performance of its TCP-HF (hexavalent-free) and TCP-NP (no-prep) room-temperature anodic seals in independent third-party testing.
Read MoreNon-Cyanide Copper Process Plates Directly onto Zinc Die Cast
At Sur/Fin 2018, EPI will highlight its E-Brite 5.0 CU alkaline non-cyanide copper process for barrel plating directly onto zinc die cast, as well as a number of other offerings.
Read MoreFinishing Options Include Hex-Chrome Alternatives
At Sur/Fin 2018, Pavco will showcase metal finishing systems for alloys, zinc, nickel, chrome, copper and conversion coatings, with an emphasis on decorative hexavalent chrome alternatives and general compliant chemistries.
Read MoreDrop-In Liners Protect Plating Tanks
Among the different material formulations that Witt Lining Systems will display at Sur/Fin 21018 are Koroseal PVC drop-in liners coupled with LFP CrossFilm skirts, designed to provide maximum corrosion protection for hard-chrome plating tanks.
Read MoreUyemura Showcasing Hard Silver, Cyanide-free, Other Plating
Uyemura will showcase a number of products at Sur/Fin 18, including Arguna 630, a hard silver electrolyte with hardness of 120-130 HV, well-suited for high-stress electromechanical components.
Read More