racking
Removing Air Bubbles
Question: I am having problems eliminating air bubbles in radiator support which have 90- degree angles.
Read MoreSubstituting Powder Coating for a Specific Standard
Question: This may be a dumb question.
Read MoreStripping Hangers
Question: I use steel angles as part of a racking system to horizontally coat aluminum extrusions with high-performance, high-temperature materials.
Read MoreColor Variation of Hardcoat Anodized Cylinders
Question: We have been getting our 6061 pressure cylinders for oceanographic instrumentation hardcoat anodized, but we have had some problems with the appearance of the finish.
Read MoreStray Currents In Copper Tank
Question: We use a copper cyanide plating bath that is “housed” in a steel tank.
Read MoreAnodic Coating on Rough vs. Smooth Substrate
Question: I am hard anodizing a 7075-T6 hot-forged part for an M-16 machine gun that has the internal cavity and some external features machined prior to anodizing.
Read MoreCleaning Larger Parts
Question: I am wondering what the best way would be to minimize process/cleaner dragout on a continuous conveyor (no indexing allowed) that is used to clean parts that are, in some cases, longer than the stage itself.
Read MorePretreatment Makes Vending Machine One Tough Customer
Fawn Manufacturing's vending machines needed a finish that could withstand harsh climates, rugged weather and tough customers. It found a pretreatment package it liked and made it better, which made for a high-quality, durable powder coating finish that stood up to the most demanding environments....
Read More